hi,i am new here , i got a question about Duromer , can someone describe its molecule structure and their characteristic?
or show me the website i can find more info about it ? thansk
 
It is not a substance, so it has no molecular structure to describe.

If it is spelt with a capital "D" It is the name of a company here in Sydney Australia. We compound engineering plastics.

If it is spelt with a small "d" it is a measurement of surface hardness, whereby the distance a specified ball can embed into the surface of a material at a specified force (or the distance might be fixed and the force measured). It's been to long since I did it.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Hi maddog153,

imho there is another meaning of duromer. It is used also for heavily crosslinked polymers, usually handled as liquids with a hardener/crosslinker. Think phenolic resins (Bakelite), epoxi resins, hard rubber (ebonite). It was the main polymer material early last century before thermoplastics came up but is still an important class of materials.

HTH Berti
 