Hello every one can any one tell me what is 5L stands for in API 5L standard

Best Regards
Zebmahar
 
Same as A106 in ASME. It defines a grade of material!!! Simples!!!
 
zebmahar (Materials)

B31.3 Ferrous, ASME B31.3, 2008, API 5L:
Type/Grade
A, B, X42, X46, X52, X56, X60, X65, X70, X80
 
Yes; "5" for Committee 5 OCTG (oil country tubular goods) and L for line pipe. Formerly there was 5L with grade A and B; and a second spec ,5LX ,containing X42 and higher strengths. These were combined into a new 5L. No user used Grade A but the mills insisted it stay in the spec.
Other Com. 5 specs; 5D- drill pipe, 5CT- Casing and Tubing.
 
thanks blacksmith37 its a very clear explaintation of my question thanks alot

Regards
Jahanzeb
 