Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

what is 40Cr10 Material

Status
Not open for further replies.

ushang70

Mechanical
Oct 11, 2003
7

Dear,
It is my first question in this Forum, we are saw pipe manufacture and for expander machine we require to develop different size of tools for respective size of pipe, our technical people are asking me to use 40cr10 material for these types of tool. I do not have much more information about this material so please if any body have any idea about it then reply for following queries.

What is 40Cr10 Material? Is it tool steel, Die steel or low alloy steel? Which heat treatment is good for this type of material?
 
Replies continue below

Recommended for you

40Cr10 is Romanian standard. its American equivalent is 5140 and material number is 1.7035

in key to steel book it is categorized as Structural and constructional steels.

the heat treatment depends on what you expect from this material.

hope it helps.
 