TJHAK
Mechanical
- Apr 14, 2010
- 6
I have a base material of SA-203 E on a vessel that I need to add a section of SA-240 304L. I am trying to write a WPS for GTAW & SAW processes for making the girth welds. I have been told by my welding consumable vendors that ER309L wire will not suffice due to the 3.5Ni content of the SA-230 E. If not, what filler metals are acceptable with both base metals? Any help or advice will be greatly appreciated.