The SJI mentions fillers and how they are able to alter the effective slenderness ratio used for analyzing a member in compression. I am particularly looking at the bottom chord panel case where it is in compression in the uplift case. I can't find anywhere online what a filler looks like. My interpretation is that these fillers help the individual member from local buckling which is why SJI offers kls/rz for two shapes with fillers or ties, where ls is the distance from panel point to filler. I am assuming it's just a plate or some sort of member that connects two members together?

Thanks in advance

1741962489150.png
1741962092240.png

1741961126432.png
 
Replies continue below

Recommended for you

Isn’t a filler just bar material—usually discontinuous—between the angles?
 
Isn’t a filler just bar material—usually discontinuous—between the angles?
that would make sense, what are their typical spacing so that we are allowed to assume they help the two angles from buckling individually? (every midspan between panel pts?)
 
agreed, a short length of rod welded between the two chord angles.
I`m accustomed to seeing them midspan between panel points, typically just a couple near the center.
Here's a couple at the top chord:
1741978499354.png
 
that would make sense, what are their typical spacing so that we are allowed to assume they help the two angles from buckling individually? (every midspan between panel pts?)
Answer is in your OP. Space based on slenderness ratios; design for 2% of axial force.
 