Anyone give me an equivalent AISI steel to the above please? Also known as 22NiMoCr47. Thanks
 
Replies continue below

Recommended for you

Sorry but there is no direct equivalent.

Analysis is as follows; -
C 0.17/0.27 - Si<=0.04 - Mn 0.5/1.0 - P&S <=0.035
Cr 0.3/0.5 - Mo 0.5/0.8 - Ni 0.6/1.2

 