May 18, 2003 #1 algeee Mechanical Joined May 18, 2003 Messages 2 Location NZ Anyone give me an equivalent AISI steel to the above please? Also known as 22NiMoCr47. Thanks
May 19, 2003 #2 mqas Materials Joined May 17, 2003 Messages 55 Location IN Sorry but there is no direct equivalent. Analysis is as follows; - C 0.17/0.27 - Si<=0.04 - Mn 0.5/1.0 - P&S <=0.035 Cr 0.3/0.5 - Mo 0.5/0.8 - Ni 0.6/1.2 Upvote 0 Downvote
Sorry but there is no direct equivalent. Analysis is as follows; - C 0.17/0.27 - Si<=0.04 - Mn 0.5/1.0 - P&S <=0.035 Cr 0.3/0.5 - Mo 0.5/0.8 - Ni 0.6/1.2