Weldolets and ASME B31.4

Status
Not open for further replies.

herriotwatt

Materials
Joined
Apr 5, 2006
Messages
1
Location
CA
Does anyone know if ASME B31.4 allows the use of weldolets as branch fittings?
 
Yes, per ASME B31.4 section 404.3 "Intersections". Review this entire section carefully to check for proper area reinforcement. Also, make sure the weldolet is properly specified for the pressure/temperature rating for your application. I would suggest visiting the web site below for additional information on weldolet fittings;

 