Depth to width ratio of stainless Steel welding decrease with increasing arc length. What is the reason for that. Any thoughts?
 
Replies continue below

Recommended for you

As the arc length increases it gets wider which spreads out the heat, resulting in a softer arc with less penetration.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
What he said!

Best regards - Al
 
Yup, and not just for stainless steel.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Thank you , Ed stainless, gtaw and ironic metturgist
 