Jul 1, 2020 #1 nabeel3 Mechanical Joined Dec 14, 2006 Messages 146 Location SA Hello Depth to width ratio of stainless Steel welding decrease with increasing arc length. What is the reason for that. Any thoughts?
Hello Depth to width ratio of stainless Steel welding decrease with increasing arc length. What is the reason for that. Any thoughts?
Jul 1, 2020 1 #2 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA As the arc length increases it gets wider which spreads out the heat, resulting in a softer arc with less penetration. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
As the arc length increases it gets wider which spreads out the heat, resulting in a softer arc with less penetration. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Jul 1, 2020 #3 gtaw Structural Joined Feb 10, 2006 Messages 1,988 Location US What he said! Best regards - Al Upvote 0 Downvote
Jul 2, 2020 1 #4 Guest Yup, and not just for stainless steel. "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
Yup, and not just for stainless steel. "Everyone is entitled to their own opinions, but they are not entitled to their own facts."
Jul 7, 2020 Thread starter #5 nabeel3 Mechanical Joined Dec 14, 2006 Messages 146 Location SA Thank you , Ed stainless, gtaw and ironic metturgist Upvote 0 Downvote