i have to establish a WPS as per ASME secIX for the following material,
API 5L x65 To SA694 F65
And
SA333 Gr 6 to SA694 F65
i have establish the single Procedure by Welding root GTAW ER 80 S2 and Other passes SMAW E-8018 G for the above two set material .
is ok as epr ASME SEC IX