I have some mechanical damage to repair on X65 material, using GTAW would I simply set away with using an ER70s filler wire?the material is 1" Thick and the scarring is vey shallow.
thanks ibn advance
 
Replies continue below

Recommended for you

Yes. For repair less than 20% of wall thickness, I would suggest ER70 S-2 filler metal. Prepare the weld repair region by removing any sharp corners, use a local preheat of 200 deg F and stringer beads. Slow cool, blend grind and perform a post repair NDT using either Liquid Penetrant or wet fluorescent MT for final acceptance of the repair area.
 