You should NOT use this filler metal for joining 304 to AR plate. The AR (abrasion resistant) plate is a low alloy steel, and using a carbon steel filler metal, such as ER70S-6, will result in cracks after solidification.
You need to use either ER 309 or Inconel (Ni-base filler metal).