What is the history behind limiting heat input to 60kJ/in the welding of stainless steel (TP 304) to prevent sensitization/ maintain corrosion resistance in the as welded condition? Is it related to grain growth or ferrite?

Thank you in advance.
 
Browse Special Metals, Outokumpu, and Allegheny Ludlum's websites. There's a ton of stuff out there.



Mike Halloran
Pembroke Pines, FL, USA
 
The heat input is limited to reduce sensitization affects, which results in reduced corrosion resistance.
 
Along with this remember that you need excellent gas coverage and an overalloyed filler.

= = = = = = = = = = = = = = = = = = = =