I apologize if this is a redundant post, but I need to specify the proper electrode for welding a 3/4" diameter stainless steel rod (304) to a schedule 40 steel pipe. This will be done in the field and is part of a life line attachment.
 
Replies continue below

Recommended for you

Usually the filler metal used for weld SS to CS would not work well with whipping. whipping is a technique used with certain fast freeze steel electrodes.

Whipping can be done with SS electrodes but the arc is just NOTHING like an E6010 or 6011.

Depending on the application, the mixture may not be a problem.



Gerald Austin
Iuka, Mississippi
 
JLG III,

Can you explain/describe what you mean by "whipping"?
 
JLGIII
I think I understand (at least in principal) what you were trying to accomplish, but, relying on whipping to avoid zinc contamination sounds like a dangerous practice.
 