Hercules28
Materials
- Nov 9, 2010
- 169
Dear all,
I am welding 304L Stainless on 304L with a 308 filler. (TIG)
I get various rainbow colors. I know that brown to white means low to high Temp exposure.
But what does the blue mean?? Does it have to do with the quality of the argon?
Thanks,
Herc
I am welding 304L Stainless on 304L with a 308 filler. (TIG)
I get various rainbow colors. I know that brown to white means low to high Temp exposure.
But what does the blue mean?? Does it have to do with the quality of the argon?