metaleng123
Petroleum
Hello everyone,
I have to write a welding tehnology for some parts that must be guaranteed at -60(-76 F). To give you some information, there will be both butt welds and fillet welds and the thickness will range between 10-20 mm( 0.39" - 0.78"). I usually weld this type of material(PNo.1) without any preheat. Considering the fact that this project has some special requierments should i take more precautions and add preheating?
Best regards,
S
I have to write a welding tehnology for some parts that must be guaranteed at -60(-76 F). To give you some information, there will be both butt welds and fillet welds and the thickness will range between 10-20 mm( 0.39" - 0.78"). I usually weld this type of material(PNo.1) without any preheat. Considering the fact that this project has some special requierments should i take more precautions and add preheating?
Best regards,
S