we have 2mm thickness RA602 CA (UNS N06025) sheet to be welded. The filler wire ERNiCrFe-12 is not available in the region. Can weld using ER NrCrMo-3 which is higher strength filler?
 
It can and has been done. You could also use ERNiCRMo-4 or ERNiCrMo-10.
 