May 31, 2019 #1 adyard Mechanical Joined Sep 7, 2011 Messages 9 Location IN we have 2mm thickness RA602 CA (UNS N06025) sheet to be welded. The filler wire ERNiCrFe-12 is not available in the region. Can weld using ER NrCrMo-3 which is higher strength filler?
we have 2mm thickness RA602 CA (UNS N06025) sheet to be welded. The filler wire ERNiCrFe-12 is not available in the region. Can weld using ER NrCrMo-3 which is higher strength filler?
Jun 7, 2019 #2 weldstan Materials Joined Jun 24, 2011 Messages 2,809 Location US It can and has been done. You could also use ERNiCRMo-4 or ERNiCrMo-10. Upvote 0 Downvote