Welding Q&T 4340 to Carbon Steel, As Welded, Asking for Advice/Feedback 1

Status
Not open for further replies.

PressEquip

Civil/Environmental
Joined
Oct 26, 2009
Messages
35
Location
CA
Thank you in advance for your time and potential responses

At the shop they repair equipment used at the facility. In this case it is a fork lift. There is pivot point (pin with a bushing), that eventually develops a flat spot (especially on the ones from the factory which are mild steel). The pin is welded to an axle that has rubber seals. In the past the shop has upgraded these weld-on pins to 4340 on several of the fork lifts. Hardness measurement was taken of one of the replacement 4340 pins: 297 HB (~31 HRC). This hardness leads me to thinking the material is quenched and tempered (such as A434 4340 BC or A434 4340 BD). They had a sample of the machined upgraded part which they showed me. On the sample, the contact surface with the bushing was discolored due to what we suspect was localized heat treatment to create a case hardened region to prolong the life of the pin. This localized hardening was probably either induction or direct flame hardening. A hardness measurement was taken on the dis-colored surface: 380 HB (~ 41 HRC). Unfortunately there isn't any documentation on record that I'm aware of such as the MTR or details on the case hardening heat treatment.

The replacement part is ~4.125" OD at the shoulder, then reduces to ~3"OD at the bushing mating surface, over-all length ~3.625".

I talked to the shop welder who usually does the welding on the fork-lifts. Since the pin is welded to an axle that has rubber seals, he only does a min. 250°F pre-heat so as not to damage the seals. The shoulder allows for up to ~0.75" leg fillet weld. The factory weld is much smaller but the mechanics manager told the welder to put on as large of weld as possible, so it is now a much larger fillet weld. They have done this repair on several fork lift and it has held up fine for years, no cracks or issues that I was told about.

I'm concerned that if the case hardening is direct flame that the surface of the part could become decarburized, induction hardening would be preferred in my opinion.

The bushing is a soft material such as bronze and there is grease channels in bushing and a grease nipple to supply grease to the bushing.

Ideally the welding procedure should be changed to have a higher pre-heat (min. 600-800°F) and post heat (min. 800°F) but that would require the rubber seals to be removed and then re-installed which is a significant amount of work.

Please provide feedback on the following:

1) Does it even make sense for the replacement pin to be case hardened in the contact region with the bushing?

2) Are there economical ways to improve this repair process?

3) Since the shop has been successful with previous repairs using the above method, is that proof enough or should certain aspects of the repair process be changed? I'm specifically thinking of the welding procedure.

If you have any questions or want clarification please request that information in the responses

Thanks


A Fan of EngTips, share the knowledge
 
31HRC is bar condition for machining. It is not hardened.
 
well it is not fully harden but it is heat treated. but yes generally it is for machinability harden.
if it works don't mess with it
 
No one is going to complain until something breaks. No one is likely to bring legal action until someone gets injured.

There are too few details in this post to make useful recommendations.

I would find it difficult to defend the "procedure" mentioned in this post, but I would find it easy to find fault with what has been described. In this case, I would rather be retained by the plaintiff than the defendant.

Best regards - Al
 
a fork lift is used to move material and equipment. it is not for lifting humans. from the description the shop is improving a faulting design.
I used a fork lift as a youngster, picking up pallets of material. no one is suppose to be under the lift, period. safety rule is no one should be under material being lifted.
based on that it is not used for lifting humans. if it breaks there may or may not be damage to material or equipment, that is on the shop Forman.
 
Thank you to all who responded. Time will tell how the repaired fork lifts perform.

A Fan of EngTips, share the knowledge
 
Without sufficient information provided, I would have likely recommendd buttering the 4340 pin with E7018 or similar filler metal using higher preheat and followed by a dehydrogenation heat treat ment at 600F for 1 hr. Then I would make the strength weld to the butter and the low carbon steel with a 200F to 250F preheat. I have used this process for similar welds with success a number of time for more than 40 years.
 
You seem to be out of your depth here.

Ask a proper welding engineer - one with metallurgical knowledge, as opposed to a structural engineer.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Brilliant suggestion weldstan! Thanks again to all who responded

A Fan of EngTips, share the knowledge
 