Good afternoon all,
As I understand, many API 5ksi flanges are made of SA105 materials. I plan to have welders weld this to A106 grade B line pipe to transition from from API wellhead to B31.3 flow line.
the WPS has the following essentials, and other variables are:
Root is MIG
fill/cap is 7018 (low hydrogen)
Pre-heat minimum is 175 F
PWHT is 1125 +/- 25F
P1 to P1
thickness range for base metal from 0.1875" to 0.944"
etc.
Can this variables be used to join an API 5ksi (SA 105) material to an A 106 grade B in the shop? as long as the two pipes meet the variables like thickness range, strenght of material, etc. This is a qualified WPS.
Thank you.
As I understand, many API 5ksi flanges are made of SA105 materials. I plan to have welders weld this to A106 grade B line pipe to transition from from API wellhead to B31.3 flow line.
the WPS has the following essentials, and other variables are:
Root is MIG
fill/cap is 7018 (low hydrogen)
Pre-heat minimum is 175 F
PWHT is 1125 +/- 25F
P1 to P1
thickness range for base metal from 0.1875" to 0.944"
etc.
Can this variables be used to join an API 5ksi (SA 105) material to an A 106 grade B in the shop? as long as the two pipes meet the variables like thickness range, strenght of material, etc. This is a qualified WPS.
Thank you.