Steelforbrains
Mechanical
What type of weld preparation would you recommend for butt welding two 1" thick A36 plates that are 48" long, I am looking for full penetration. I am using flux cored 0.065 wire. What would be the minumum groove size and can I get away without preheating. As always I am limited on fabrication time so the quicker and dirtier the better.
Thanks
What is a good source for information like this?
Thanks
What is a good source for information like this?