Gents,Have to weld a 12 inch sch.120 pipe P1 to P1,can't pwht due to poor engineering design. Won't bore you with details. Would like to weld with inco 82. 1)Butter with inco,maintain 200F preheat,max interpass 350F using narrow weld beads to include HAZ 2)Blend butter passes with flapper and PT. 3) Fill remainder of joint with inco 82.Have also considered temper bead. B31.8 requires no pwht for this wall thickness,b31.3 does require pwht which is the code I'm bound too. Two questions,
Good or bad idea using the inco in lieu of pwht? Any clue why one code requires pwht and the other does not? I'm no metallurgist so if i'm missing the boat feel free to point it out. thanks
Good or bad idea using the inco in lieu of pwht? Any clue why one code requires pwht and the other does not? I'm no metallurgist so if i'm missing the boat feel free to point it out. thanks