atomicbob
Industrial
- May 5, 2008
- 8
We recently discovered a supplier had substituted B7 studs in place of the SA36 we ordered. (a no charge "upgrade") Some of these B7 studs got welded to SA516-70 plate as a lifting device (GMAW ER70S-6). I know that ASME does not recognize B7 as a weldable material, but this is not an ASME Code weld. It just needs to work. I am not concerned with the diminished tensile strength of the stud materials as it is not under high load. Perhaps 500 pounds on a 1" stud.
The question I have is, are these welds mechanically sound? Or is the B7 so hard that it will simply crack at the heat affected zone under impact? Or...???
Many of them are in the field and replacement would be difficult to replace.
Thanks
The question I have is, are these welds mechanically sound? Or is the B7 so hard that it will simply crack at the heat affected zone under impact? Or...???
Many of them are in the field and replacement would be difficult to replace.
Thanks