I am required to install a 2-63mm x 63mm x 100metre billet for an overhead crane rail. This is to be welded into a crane rail beam. Can someone please provide some advise on the following issues:
What are the acceptable welding procedures? I am told of 3 methods - Thermic, puddle arc and flash butt.
Is fillet weld to the beam sufficient?
Is preheating mandatory? Some say this will cause misalignments
How to weld the joints? Is cut square or bevelled acceptable?
Is weld required for the full cross sectional area of the joint?
What are the welding tests required?
This is only a 15T crane. Any quick but proper solution to accomplish this?
Thanks.
What are the acceptable welding procedures? I am told of 3 methods - Thermic, puddle arc and flash butt.
Is fillet weld to the beam sufficient?
Is preheating mandatory? Some say this will cause misalignments
How to weld the joints? Is cut square or bevelled acceptable?
Is weld required for the full cross sectional area of the joint?
What are the welding tests required?
This is only a 15T crane. Any quick but proper solution to accomplish this?
Thanks.