ASTM A532 Grade IIIA. Any hope at all of welding this?

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
 
Doubtful.

Best regards - Al
 
Thanks Al. I was pretty certain, but I have seldom encountered any kind of cast iron welding.

This question was really for that one guy in the room who will claim that anything can be welded. I'm sure you've met him.

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
 