how to weld hardox 400 materials

which consumable can use hardox 400 materials
 
It welds with your standard 7018 electrodes or S2 wire. It may require preheat.
 
E7018 Electrode to meet tensile strength of Hardox 400 materials
 
Generally, these wear resistant alloys are being welded to lower strength structures so there is no meed for the weld to exceed the strength of the structure.
 
Hi, Please see the following Welding Hardox guide for the information you were looking for: If you have any further questions, please feel free to contact one of our Technical Development Managers, they are there to help exactly with these types of questions, you can reach them by completing this form:
All the best!
 