Hello,

In this thread ( metengr asserts that "it is not permitted to be welded under ASME B&PV Code" relative to ASTM A193 GR B7 material. I tried to find the clause but wasn't able to.

Does anyone know what specific clause of ASME B&PV prohibit the welding of this steel?

Thanks.
 
A193-B7 bolts are heat treated that is why you shouldn't do any welding on it.
 
For "specific clause", it might state something to that effect in the A193 spec.
Or it could just be a practical issue of not being able to qualify a weld with the material.
Or it could be that the material is not listed under the different base metals.
 
This is a thread fixing system, why not continue with it? Why weld it?

Regards
 
I don't think you are allowed to modify the material of the bolting in any way without compromising the certification of the bolt to the ASTM A193 standard.

ASTM A193 references A962, which states under 16 Retests and rework: "16.3 Repair by welding is prohibited".
 
Thank you guys for you answers.

I asked this question only because of curiosity and not because i have a need to weld A193 Gr. B7 steel. I ended up reading the thread and saw the response but couldn't find the specific clause and asked here.
 
Not in ASME but stumbled on this in API 560 today

12.5.6 If the minimum service temperature is –18 °C (0 °F) or higher, bolting material shall be in accordance with
ASTM A307, ASTM A325, ASTM A193-B7, or equivalent. Below –18 °C (0 °F), A193-B7 bolts with ASTM A194-2H
nuts, ASTM A320-L7 bolting, or equivalent shall be used. No welding is permitted on A320-L7 or A193-B7 materials.
 