I am in the process of designing a part made form M-2 tool steel, which will need to be welded. I will have two tubes 0.600" in diameter with 0.050" wall thickness. The tubes will be "butted" together with a small overlap on the I.D. for centering then welded. The welding will be done pre heat treatment.
From what I can find, I will need to pre-heat the parts to above 200F and use a rod that has material properties similar to M-2 when heat treated. I am planning on having the parts TIG welded. Is there a good resource for welding rod type, pre-heat temp, post weld cooling, etc. for dealing with M-2 tool steel? Has anyone had any experience with welding M-2? Thanks for the help.
Dan
From what I can find, I will need to pre-heat the parts to above 200F and use a rod that has material properties similar to M-2 when heat treated. I am planning on having the parts TIG welded. Is there a good resource for welding rod type, pre-heat temp, post weld cooling, etc. for dealing with M-2 tool steel? Has anyone had any experience with welding M-2? Thanks for the help.
Dan