Is it acceptable to weld Incoloy 825 to 316 together? I know that's a broad term, but any information would be appreciated. Can anyone offer any advice on, or references for welding disimilar metals like this?
 
Replies continue below

Recommended for you

This type of weld can be done and is done using a Ni-base filler metal. Heat input during welding is important as well as joint cleanliness. I would recommend you visit the Special Metals web site below, and review their technical information on welding/joining;

 
They are frequently welded together with E/ERNiCrMo-3. Other nickel base alloy filler metals are also employed.

 
this publication from Nickel Institute can give you some good advice on dissimilar welding.

14018 - GUIDELINES FOR WELDING DISSIMILAR METALS (1991)
By Richard E. Avery, reprinted from Chemical Engineering Progress, May 1991. Nickel-containing stainless steels and nickel- and copper-base alloys are readily fusion welded to carbon and low-alloy steel and to each other. Methods are described to estimate the weld metal composition of dissimilar-metal welds. Knowing the composition, weld properties can be predicted for a wide range of dissimilar-metal welds.

hope this help

S.

 