Hello All,
Our client is connecting two screw piles by welding a collar (sleeve) into it. However they were doing this welding when outside temperature was around -30 0C below.
After our repeated screaming, contractor began to weld in a covered tent. Can anyone tell me where I can find answers to following questions;
1. Does the contractor requires to preheat the weld area? if so what temperature?
2. Does the inter-pass temperature has to be high? what temperature?
3. Does the contractor requires to use a blanket to wrap up weld area? at what temperature he has to cover with a blanket and remove?
4. What is the minimum temperature that welding cannot be done?
Thanks in advance.
Our client is connecting two screw piles by welding a collar (sleeve) into it. However they were doing this welding when outside temperature was around -30 0C below.
After our repeated screaming, contractor began to weld in a covered tent. Can anyone tell me where I can find answers to following questions;
1. Does the contractor requires to preheat the weld area? if so what temperature?
2. Does the inter-pass temperature has to be high? what temperature?
3. Does the contractor requires to use a blanket to wrap up weld area? at what temperature he has to cover with a blanket and remove?
4. What is the minimum temperature that welding cannot be done?
Thanks in advance.