I have specified galvanized steel and a steel roof deck over a wash bay. On site, the Superintendent mentioned that the welder has raised concerns over the fumes produced by puddle welding the steel deck. The Superintendent also said that the burn through compromises the galvanized coating on the underside of the deck.
I’ve been looking online but I have not really seen anything about the issues of welding galvanized deck. Are the fumes still a concern if the welding occurs on a roof deck? Is it typical to just call up Hilti pins instead?