Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

welding galvanized members

Status
Not open for further replies.

v2

Structural
Joined
Jun 2, 2002
Messages
95
Location
US

is it ok structurally without affecting the connection strength to weld hot dipped galvanized HSS together?

what I should be concerned about in either case?

thank you
V2
 
When you weld galvanized steel, remove the protective coatings next to the haz zone, thus leaving a raw, unprotected area in the weld zone. This precautions must be taken to avoid porosity and cracking of the weld caused by penetration of zinc into the weld pool while using arc and oxyfuel processes. Cold Galv can be applied after the welding.

Adequate ventilation combined with proper fume extraction will completely eliminate exposure to welding fumes.
 