I recently inherited some new work, that being to write and coordinate qualification of weld procedures. And I have two basic question that I hope to get your advice on:
1. On some of the old standard forms for our procedures, there is a block for "Calibration Procedure" which has typically been left blank. My question is, do the welding machine power supplies or transformers require calibration by Code (any) or is it standard shop practice to do so? Or is it never done (which appears to be our case)?
2. Should a weld procedure be qualified for the specific machine owned by the shop? In other words if we own Lincoln and Hobart TIG machines, is there a requirement to do qualify the procedure twice (once with each machine)?
By the way, we do Mil Std NAVY) and AWS welding.
Thanks in advance.
TC
1. On some of the old standard forms for our procedures, there is a block for "Calibration Procedure" which has typically been left blank. My question is, do the welding machine power supplies or transformers require calibration by Code (any) or is it standard shop practice to do so? Or is it never done (which appears to be our case)?
2. Should a weld procedure be qualified for the specific machine owned by the shop? In other words if we own Lincoln and Hobart TIG machines, is there a requirement to do qualify the procedure twice (once with each machine)?
By the way, we do Mil Std NAVY) and AWS welding.
Thanks in advance.
TC