1.Kindly teach me regarding the welding joint detail for 36mm thk shell plate (316L) of 900 # vessel.

2.If the lifting lug is touching the capping of the welding joint b/w ellipsoidal head and shell of the vessel,than is it allowed to flush the capping to keep the lifting lug straight?Vessel is 800 mm od and TTL is approx.2.8m and 900 #.

Regards.
mechanical19k96@hotmail.com
 
Replies continue below

Recommended for you

If you mean the weld joint detail used during fabrication of the vessel shell welds, the answer is that they should be full penetration welds with a joint configuration of a single-vee or double-vee configuration.

Yes, the weld cap can be ground flush to improve fit-up with a lifting lug.
 