Dear My Friends,
My project have to qualify 1 PQR between Super Duplex A790 UNS 32750 to Super Duplex A790 UNS 32760. Mechanical test require:
1. Pitting Corrosion at 40 Degree (No Pitting)
2. Range Ferrite: 35-65%.
3. Max Hadness 350 HV10
I am wondering which consumable we should use, ER2594 Metrdoe 2507 or ER2594 Metrode Zeron 100X.
What is different between metrode 2507 and metrode Zeron 100X. Pls give your recommendation.
My project have to qualify 1 PQR between Super Duplex A790 UNS 32750 to Super Duplex A790 UNS 32760. Mechanical test require:
1. Pitting Corrosion at 40 Degree (No Pitting)
2. Range Ferrite: 35-65%.
3. Max Hadness 350 HV10
I am wondering which consumable we should use, ER2594 Metrdoe 2507 or ER2594 Metrode Zeron 100X.
What is different between metrode 2507 and metrode Zeron 100X. Pls give your recommendation.