daniel1978
Mechanical
Guys
we are in middle of our TA, in one of our vessel (non pressure tower) i need to weld few clips ( to be permanent) however vessel plate is explosion bonded. so i have few questions to ask:
1- i assume we cant weld to EB plate ?
2- i ask foreman to grind the plate to get in to original plate then weld all clips and repair the cladding. is this correct action item?
3- repair locations has repair cladding does this repair make any issue in future ? (this will not the same as explosion bonding process) quality of cladding is not the same.
appreciate for your quick response
we are in middle of our TA, in one of our vessel (non pressure tower) i need to weld few clips ( to be permanent) however vessel plate is explosion bonded. so i have few questions to ask:
1- i assume we cant weld to EB plate ?
2- i ask foreman to grind the plate to get in to original plate then weld all clips and repair the cladding. is this correct action item?
3- repair locations has repair cladding does this repair make any issue in future ? (this will not the same as explosion bonding process) quality of cladding is not the same.
appreciate for your quick response