Hi,
I'm installing a roll cage in a race car. I'm using ChromeMolly (spelling?) 4130. I was planing on using ER80S-D2 filler rod, but the box was labled wrong and I was given ER80S-B2 Filler rod instead. I have welded about 1/4 of the bar in. I now have the correct filler rod, but my question is, am I ok with what I welded so far? Or do I need to cut out what I've welded and start over.
Thanks in advance.
SCott
I'm installing a roll cage in a race car. I'm using ChromeMolly (spelling?) 4130. I was planing on using ER80S-D2 filler rod, but the box was labled wrong and I was given ER80S-B2 Filler rod instead. I have welded about 1/4 of the bar in. I now have the correct filler rod, but my question is, am I ok with what I welded so far? Or do I need to cut out what I've welded and start over.
Thanks in advance.
SCott