Gentlemen
The cast iron repair job is the 100 year old arms of old Yorkshire Signposts. My painting Team are shotblasting and painting them but a good number are cracked or broken due to vehical damage and have been repaired many yrs ago by mechanical straps or even very primitive weldingthat has failed. , but, yes, it is gray !!WE don't have a spec for the CI.
On advice from chicopee we braized a couple today - - (We have a very skilled welder in our W/S ) Our test is very non scientific. We lay the arm flat across two bricks then jump on it, hard. So far we are 100% sucessfull - - no breaks. My fear is that one day a heavy arm might break and fall on someones head !! We paint the arms so visual is of no importance and I guess paint keeps joint dry from rain so dissimilar metal corrosion will be no bother (I hope)
Gents, I greatly appreciate all your comments- - I guess its the Learning Curve again.
Please feel free to shout at me if I am doing anything daft
Corrosionman