Hi,
I need to weld a fitting made up of CA-40 (Martensitic stainless steel) material to carbon steel (A106) pipeline. The fitting end connection size is 25NB Socket Weldable.

I’m looking for the advice on the following:
• Welding consumables (SMAW)
• Recommended Preheat Temperatures
• Recommended PWHT procedure
• Any other Do’s and don’ts

Thanks in advance.
 
Replies continue below

Recommended for you

blacksmith,

Thanks for your response.
Brazing won't be acceptable in this case and welding process is mandatory.
 