In the A606 specification two conditions are noted for this steel, "as-rolled" and annealed; the mech. properties of annealed are about 10% less than as rolled. I am concerned that welding as-rolled material alters the properties to the annealed values in the HAZ. Does anyone know if this is true?

BATman2

 
Replies continue below

Recommended for you

Don't worry. Welding of hot rolled A-606 will not "anneal" the HAZ to the lower strength of annealed A-606.

 
Stanweld,

Thanks. What's curious is why AWS D1.1 only reports the annealed values for A606 in the material tables.
 
AWS D1.1 is simply giving the minimum strength of A-606 since there are no "grade" designations.

 