I am in need of specific examples of structural failure that could be attributed to welding and welding defects.

Does anyone know of links that they could provide?

Thanks in advance.
 
Replies continue below

Recommended for you

Try to get hold Northridge Earthquake Structural Failure Investigation Report. It was put out by AWS. It has numerous weld faliures with analysis.
 
Nice photographs Metengr!

Best regards - Al
 