I am in need of specific examples of structural failure that could be attributed to welding and welding defects.

Does anyone know of links that they could provide?

Thanks in advance.
 
Try to get hold Northridge Earthquake Structural Failure Investigation Report. It was put out by AWS. It has numerous weld faliures with analysis.
 
Nice photographs Metengr!

Best regards - Al
 
I added metengr's picture site to my favorites list.
 