ColonelSanders83
Mechanical
- May 11, 2009
- 236
Hello All,
I have suddnely found myself needing to weld a few sock-o-lets to a couple of ammonia lines. Apparently the holes have already been cut in the lines and I have been requested to evaluate the use of Argon as a backpurging gas in the pipe to perform the welding. Apperently there is a small risk there may still be a small amount of ammonia vapor present. Normally I would use nitrogen to purge out the system, but since they have plenty of Argon at site thats what they would like to use.
A google search on the subject came up dry, so I was wondering if any of the more experienced folks here could offer some guidence. Are there any interaction concerns with ammonia and argon? Am I going to regret allowing (or disallowing this) in the near future? I absolutley hate to make a decision with no information. Any help or guidence or useful referances on the matter would be greatly appreciated.
A question properly stated is a problem half solved.
Always remember, free advice is worth exactly what you pay for it!
I have suddnely found myself needing to weld a few sock-o-lets to a couple of ammonia lines. Apparently the holes have already been cut in the lines and I have been requested to evaluate the use of Argon as a backpurging gas in the pipe to perform the welding. Apperently there is a small risk there may still be a small amount of ammonia vapor present. Normally I would use nitrogen to purge out the system, but since they have plenty of Argon at site thats what they would like to use.
A google search on the subject came up dry, so I was wondering if any of the more experienced folks here could offer some guidence. Are there any interaction concerns with ammonia and argon? Am I going to regret allowing (or disallowing this) in the near future? I absolutley hate to make a decision with no information. Any help or guidence or useful referances on the matter would be greatly appreciated.
A question properly stated is a problem half solved.
Always remember, free advice is worth exactly what you pay for it!