Jun 21, 2006 #1 metaal Materials Joined Jul 14, 2003 Messages 11 Location DE We want to weld Alloy 926 (Cronifer) onto SS316L material. Have anyone experience with this ? What precautions we have to taken ? Is PWHT needed ? What type of filler material is needed ?
We want to weld Alloy 926 (Cronifer) onto SS316L material. Have anyone experience with this ? What precautions we have to taken ? Is PWHT needed ? What type of filler material is needed ?
Jun 21, 2006 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US The information from the ThyssenKrupp VDM web site below is an excellent source of information on this alloy, including welding and filler metal information; http://www.thyssenkruppvdm.com/navi/25.htm To answer your questions; No preheat No PWHT and keep your interpass temperature below 175 deg C. Upvote 0 Downvote
The information from the ThyssenKrupp VDM web site below is an excellent source of information on this alloy, including welding and filler metal information; http://www.thyssenkruppvdm.com/navi/25.htm To answer your questions; No preheat No PWHT and keep your interpass temperature below 175 deg C.