We want to weld Alloy 926 (Cronifer) onto SS316L material. Have anyone experience with this ?
What precautions we have to taken ?

Is PWHT needed ? What type of filler material is needed ?
 
Replies continue below

Recommended for you

The information from the ThyssenKrupp VDM web site below is an excellent source of information on this alloy, including welding and filler metal information;






To answer your questions;
No preheat
No PWHT and keep your interpass temperature below 175 deg C.
 