Resulphurised steels are highly prone to hot tearing during hot forming and hot cracking during welding. You may wish to experiment by buttering a sample of the 1141 bar, to be used in production, with E7018 and confirm freedom from cracking. Then make the strength weld between the E7018 buttered bar and the plate. No guarantee that this will be successful though!!!