Welding AerMet Tool Alloy 1

Status
Not open for further replies.

MadMango

Mechanical
May 1, 2001
6,992
I need to pass a .75" OD bar of stainless 15-7 through a 1.00"thk 4.25" OD disk of AerMet tooling alloy. We then need to weld the bar to the AerMet and heat treat the whole thing to get close to RC50-55. The bar is offset from center of the disk and will act as a crank.

I am unfamiliar with this material, and am looking for advice on type of welding, and PWHT call-out on the drawing.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
Replies continue below

Recommended for you

As an update, we have abandoned the AerMet alloy and are using 15-7 across the board with PWHT to RH950.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
Thank you Metengr.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of Eng-Tips Forums?
 