We have to Weld A514 Grade Q to API 2H Grade 50 and the question is how to lower the hardness values down to 325HV without having to PWHT.because the overmatch as far as yeild and tensile strengths are considerable between the two materials we are not overly concerned with the loss of some of the mechanical properties of the A514 .
Consumable is lincoln ultracore 71A85,Trials so far have suggested a higher than normal preheat 400F with max interpass 500 and using slow higher heat input runs.
Given that the A514 material is already hitting over 300HV ,325HV is not a realistic target but we would like to find away of lowering the hardness as much as possible .Anyone have any ideas .
Consumable is lincoln ultracore 71A85,Trials so far have suggested a higher than normal preheat 400F with max interpass 500 and using slow higher heat input runs.
Given that the A514 material is already hitting over 300HV ,325HV is not a realistic target but we would like to find away of lowering the hardness as much as possible .Anyone have any ideas .