Feb 14, 2007 #1 weldgal Industrial Joined Apr 28, 2006 Messages 46 Location US Has anyone done this successfully in either the GTAW or GMAW process?
Feb 14, 2007 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US weldgal; What are we talking about 70/30 copper nickel or brass? If it is 70/30 Copper Nickel http://www.nickelinstitute.org/index.cfm/ci_id/3185/la_id/1/tecArticle/1 Upvote 0 Downvote
weldgal; What are we talking about 70/30 copper nickel or brass? If it is 70/30 Copper Nickel http://www.nickelinstitute.org/index.cfm/ci_id/3185/la_id/1/tecArticle/1
Feb 14, 2007 Thread starter #3 weldgal Industrial Joined Apr 28, 2006 Messages 46 Location US 70/30 copper nickel. Upvote 0 Downvote
Feb 19, 2007 #4 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US Assuming that HSLA-65 is equivalent to 5LX-65, we have made these sdissimilar welds using 70/30 copper nickel filler, aluminum bronze fillers and Nickel fillers. Upvote 0 Downvote
Assuming that HSLA-65 is equivalent to 5LX-65, we have made these sdissimilar welds using 70/30 copper nickel filler, aluminum bronze fillers and Nickel fillers.